When the water consumption remains constant, the slump of the concrete can be increased by 10 to 20 centimeters.
② While maintaining the workability of the concrete unchanged, the water content can be reduced by 10% to 50%, and the concrete strength can be increased by 15% to 20%. Especially, the improvement in early strength is more significant.
③ When the concrete strength remains unchanged, the amount of cement can be reduced by 10% to 15%.
④ The heat release rate during cement hydration slows down, and the peak of heat release is delayed.
⑤ The problems of concrete bleeding and segregation have been significantly improved.
⑥ The permeability of concrete can be reduced by 40% to 80%, while enhancing its resistance to water penetration, freezing, chemical corrosion, rusting and other properties.
⑦ It can be mixed with special concrete, which is more economical, simpler and more flexible than using special cement.